Toxicity Effect of Copper oxide Nanoparticles on Artemia salina

 

K. Kumaresn1, D. Parthiban1, V. Sivanarayan1, N. Arun1*, P. Kumaravel2

1Department of Biochemistry, Vysya College, Salem-103

2Department of Biotechnology, Vysya College, Salem-103

*Corresponding Author E-mail: aamaravian@gmail.com

 

ABSTRACT:

We evaluated the stability of CuO NPs, and the toxic effects of their suspensions to Artemia salina (A. salina) larvae to elucidate the chemical and toxicological impact to marine micro-organisms. The results pointed to the fact that suspensions of CuO NPs were not acutely toxic to Artemia at environmentally feasible levels. However, prolonged exposure to the same suspensions induced significant toxicity. The results revealed that CuO NPs aggregate in seawater to micrometer particles. This process would ultimately reduce the toxic properties of the NPs. Nevertheless, CuO NPs showed differences in toxic effects depending on the concentration of nanoparticles. In future studies more attention should be given to the formulations of CuO NPs to better understand their toxicological properties since both surface properties and ion release kinetics change with underlying manufacturing processes. The exposure of these A. salina larvae to the selected MO-NPs did not induce significant mortality, although the NPs accumulated in the gut. However, behavioral and chemical analysis occurred after the exposure. The swimming speed alterations represent valid endpoints for CuO NP exposure.

 

KEYWORDS: CuO nanoparticle, Artemia Salina, Enzymes, Mortality, FTIR..

 

 


INTRODUCTION:

Nanotechnology is an intensive branch of science that interesting in the materials among the size of 1-100 nm with different shapes of spherical nanoparticles, nanorods, nanoribbons, nanobelts and nanoplatelets. The unique physical and chemical properties are due to its high surface-to-volume ratio comparing with micro or bulk-size. The nanomaterials can be obtained with different methods such as solid−liquid discharge process, novel quick-precipitation and direct thermal decomposition methods.

 

Nanomaterials are now become available and useful in all the man daily life applications such as in: medicine, solar cells, water purification, pharmaceutical and catalysts. Among various transition metal oxides, copper oxide (CuO) nanoparticle has attracted greater attention due to its fascinating properties such as the basis of high critical temperature (Tc) superconductors. CuO is a semiconducting compound with a narrow band gap and is used for photo-conductive and photothermal applications. Some methods for the preparation of nanocrystalline CuO have been reported such as the sonochemicalmethod  sol-gel technique, one-step solid state reaction method at room temperature, electrochemical method and thermal decomposition of precursors. Copper can also be used as an antimicrobial agent, and CuO nanoparticles have been investigated previously for enhancing antibacterial properties.

 

The Copper oxide (CuO) is a semiconducting compound with a monoclinic structure CuO crystal also has photo catalytic or photovoltaic properties and photoconductive functionalities. There is limited information available about the antimicrobial activity of nanoCuO. It is suggested that highly ionic nanoparticulate metal oxides, such as CuO, may find potential application as antimicrobial agents as they can be prepared with extremely high surface areas and unusual crystal morphologies. CuO nanoparticles were effective in killing a range of bacterial pathogens involved in hospital-acquired infections. But a high concentration of nanoCuO is required to achieve a bactericidal effect for Biosynthesis of metal nanoparticles using plants are currently under exploration. It has received more attention as a suitable alternative to chemical and physical methods (1).

 

In some literature Cuo nanoparticle have some toxic effect. The Cuo nanoparticle capped with carbohydrates it reduces the level of toxicity. Due to the interparticle interaction such as Vander Waals force and magnetic interaction the chemically synthesized particles gets agglomerated. This agglomeration reduces the specific surface area and the interfacial free energy, thereby diminishing particles reactivity. To prevent the agglomeration, the surface of the particles was passivated through the layer of stabilizer. A stabilizer can enhance dispersion and steric hindrance. Carbohydrates can act not only as stabilizer but also as a reducing agent, leading to the formation of noble metal nanoparticles. Such conjugated water soluble nanoparticles can have potential antimicrobial applications(2).

 

Among the various several metallic oxide nanoparticles Magnesium oxide nanoparticles, Copper oxide nanoparticles, Titanium dioxide nanoparticles, Zinc oxide nanoparticles have several important applications in the field of. Biolabelling sensors, antimicrobial agents,watertreatment, synthetic textiles, biomedical and surgical devices, food processing and packaging. Moreover, the composites prepared using metal nanoparticles and polymers can find better utilization due to the enhanced antimicrobial activity. Metal oxides nanoparticles (NPs) have shown their great interest in field of sensing, optoelectronics, catalysis, solar cells and so on due to their unique physical and chemical properties differing from the bulk. The various several metallic oxide nanoparticles are Magnesium oxide nanoparticles, Copper oxide nanoparticles, Titanium dioxide nanoparticles, Zinc oxide nanoparticles have several important applications in the field of. Biolabelling sensors, antimicrobial agents, water treatment, synthetic textiles, biomedical and surgical devices, food processing and packaging. Moreover, the composites prepared using metal nanoparticles and polymers can find better utilization due to the enhanced antimicrobial activity (3).

 

Metal oxide NPs modulate the activities of various processes at cellular, biochemical and genetic level in biological systems. It includes activation of oncogenes, inactivation of tumour suppressor genes, alteration in cell cycle control checkpoints and impaired DNA repair. It is well known that unrepaired DNA damage leads to carcinogenesis. Therefore, genotoxicity assays for improved cancer risk assessment have gained momentum. Several genotoxicity assays such as Comet assay for DNA single and double strand breaks; chromosomal aberration test; micronucleus assay (clastogenic activity); sister chromatid exchange and Ames test / HPRT gene mutation assay have been applied in assessing NP induced DNA damage(4).

 

Artemia salina

Artemia salina is a primitive aquatic arthropod (salt lakes)  of the Artemiidae family  with an age of about 100 million years. Species ecology Artemia salina lives only in lakes and ponds with high salinity, which varies between 60-300 ppt. It was also discovered in Elkhorn Slough (California), which communicates directly with the sea. It is a species endemic to the Mediterranean, but is found on all continents. In our country is reported in salt lakes (Bear Lake, Ocna Sibiu, Techirghiol, Braila Salt Lake, etc.) contributing to the formation of sapropelic mud used in peloidotherapy. Artemia salina is associated with current or past commercial exploitation of salt. The Can tolerate large amounts of salt (up to 300 grams of salt per liter of water) and can live in quite different solutions of seawater such as potassium permanganate and silver nitrate. Iodine, which is found frequently in salt for human use, is harmful to this species(5).

 

These animals have the ability to reduce the osmotic pressure of haemolymph by NaCl excretion against the concentration gradient. Has been shown to developed a mechanism to maintain haemolymph extreme hypotonic in saline extreme media. Also, this species can survive in water with high oxygen deficiency. Minimum concentration of oxygen for an adult is very low, 0.5 milligrams per liter, and for naupliia even less than 0.3 milligrams per liter. Typical salt lakes have seasonal or cyclical droughts, periods when completely dry. During this process salt water concentrations ranging from ideal to barely tolerable. Larvae have only one eye (photoreceptor). Later, it developed two eyes, but the initial eye remains, resulting three eyes. Nauplia are phototactic, while adults not. They swim through the water column (phototaxis) using antennas. Mandibles are used to filter water and phytoplankton(6).

 

Artemia salina species individuals, especially in stage nauplia, are used in aquaculture as live food for commercial growth (in incubators) of many species of fish and shellfish. Resilience of these animals makes them ideal for testing samples in the experiments. Artemiasalina is one of the organisms used regularly for toxicity testing of various chemicals. Together with other bodies formed by decomposition salt lake bottom mud used to treat various rheumatic , gynecological, endocrine diseases, etc. Salt water and mud from lakeUrsuheliothermal contain hormones released by Artemiasalina: human estrogen-like SU 95%, respectively human progesterone-like 0.7 to 0.8 mg%. They are used to treat gynecological diseases: ovarian failure, infertility, etc. (7).

 

MATERIALS AND METHODS:

Chemical reagents:

The oxides of zinc and copper were synthesized using hydrated salts of zinc and copper chloride (ZnCl2 and CuCl2.H2O), methanol, sodium hydroxide, glucose which were purchased from Sigma Aldrich and used as obtained.  

 

UV-visible and FT-IR spectroscopic measurements:

The absorption spectra of ZnO and CuO were taken using aAnalytikjena SPECORD 50 UV-visible spectrophotometer and the emission spectra were recorded on a LS 45 Perkin-Elmer fluorimeter with a Xenon lamp at room temperature using methanol as a solvent in a 1-cm pathlength quartz cuvette. Surface interaction of glucose on the nanoparticles of all samples was characterized using FT-IR Perkin Elmer 100 spectrometer. Measurements were performed with manually placing the solid sample on a diamond tip and pressed for analyses. 

 

Electron Microscopy:

The transmission Electron Microscopy (TEM) and High Resolution TEM images were obtained using a JEM -2100 JEOL electron microscope. The samples were prepared by placing a drop of a dilute solution of sample in methanol on a copper grid. The samples were allowed to dry completely at room temperature. 

 

X-Ray Diffraction:

X-Ray diffraction (XRD) patterns on powdered samples were measured on Phillips X’Pert materials research diffract meter using secondary graphite monochromatic Cu Kα radiation (λ=1.54060 Å) at 40kV/50 mA. Measurements were taken using a glancing angle of incidence detector at an angle of 2º, for 2θ values over 20º-70º in steps of 0.05º with a scan speed of 0.05º    2θ.s-1.

 

Synthesis of Zinc and copper oxide nanoparticles:

Zinc and copper oxide nanoparticles were synthesized using zinc chloride (ZnCl2) and copper chloride (CuOCl2.H2O), ethanol (CH3OH), sodium hydroxide (0.10 M) and glucose. The solutions were prepared in ethanol (50 mL). To prepare 0.10 M solution, sodium hydroxide pellets were dissolved and in 20 ml ethanol stirred for 20 minutes at room temperature. Amounts of glucose were varied from 1.00 g, 0.50 g and 0.25 g for each experiment was added into the prepared solution stirring and continued further for 40 minutes. Zinc chloride (0.10 M in 20 ml ethanol) and was slowly added to this solution and stirred for 2 hours. The precipitate obtained was washed with methanol and separated by centrifuge and dried to get ZnO nanoparticles in solid form.

 

Acute toxicity test:

Materials:

        1. Saltwater

        2. Beakers

        3. Lamblight

        4. Petriplate

        5. Microscope

 

 

Produce of Artemia Salina:

Methods:

1.      12.5gm of salt and mixed with 500ml of tapwater.

2.      Then using artemia eggs ½ capsule mixed with 500ml of tapwater.

3.      Continuesly rotating the air pump motors.

4.      Then using the lamb light continuesly applied in 24 to 48 hrs.

5.      After finally hatched in artemiasalina eggs.

 

Methods:

1. 3.2gm salt was taken mixed with 20 ml of table water each petriplate.

2. Then using different concentration of copper oxide (0.5, 1.0, 1.5, 2.0 and2.5).

3 .After copper oxides mixed with stirrer 20 minutes.

4. Each petriplate added in 13 ArtemiaTerated larva .The matined   20ºC in 48 hrs.

5. This is 16 hrs light filled and 8 Dark filled.

6 .After 24 hrs and 48 hrs counted in live and death in Artemia was measured.

7. The morphology structure view microscope.

8 .After Artemia Structure observed for its malformations.

9. The Photographs were taken.

 

Swimming speed alteration test:

Methods:

1.3.2gm salt was taken mixed with 20 ml of table water each petriplate.

2. Then using different concentration of copper oxide (0.5, 1.0, 1.5, 2.0 and 2.5).

3 .After copper oxides mixed with stirrer 20 minutes.

4. Each petriplate added in 13 Artemia Teratedlarva. Thematined   20ºC in 48 hrs.

5.  This is 16 hrs light filled and 8 Dark filled.

6 . After 24 hrs and 48 hrs counted in live and death in Artemia was measured.

7. Live Artemia measure the different concentration swimming speed distance calculate in 1seconds.

8. The swimming speed value given by figure.6

 

Inhibition (%) =[(S Treated−S Control)/S Control)×100].  

 

Chemical analysis:

Method:

1. 24gm salt and 150µg of copper oxide taken mixed with 150 ml of tape water in each beaker.

2. Then using different concentration of copper oxide (150µg, 200µg, 250µg).

3 .After copper oxide mixed with stirrer 40 minutes.

4. Each beaker added in 50 Artemia treated larva and maintained 20ºC for in 48 hrs.

5. This is 16 hrs light filled and 8 Dark filled.

6 .After 48 hrs filter the artemia sample solution.

7. Then try larva was taken in 0.1gm.

8. The artemia larva how muchi taken in copper oxide.

9. Finally try larava was measured in MSP.

10. Finally value giving the result.

 

 RESULTS AND DISCUSSION

 Characteristics of Glu-CuO NP

 UV-Visible spectral analysis of Glu-CuO nanoparticles

The Glu-CuO NPs have been characterized by UV-Vis spectroscopy and spectrum is shown in figure 1. The strong absorbance peak is seen at 325 nm which is a characteristic of surface plasmon resonance of CuO NPs and therefore it shows the presence of CuO NPs. During CuO NP synthesis, D-Glucose acts as reducing agent as well as capping agent in alkaline aqueous environment due to addition of NaOH. Glucose is bound to surface of copper by hydrogen bonding of hydroxyl (–OH) group it.

 

SEM and XRD:

Figure 2 shows Scanning Electron Microscope image of synthesized CuO nanoparticle capped with glucose (0.25%). SEM provides the image of the particle revealing cubic and hexagonal shape with a diameter of 100 – 200 nm.  Carbohydrates contain many hydroxyl and carbonyl groups; these groups offer sugar coated nanoparticle a unique H-bonding capabilities in constructing supramolecular architecture.  Upon surface coating with nanoparticles they provide attractive nano construction abilities for building smart nanomaterials [Barrientos et al., 2003, Reynolds et al., 2006 and Halkes et al., 2005]. Figure 3 shows the X-ray diffraction patterns of CuO NPs capped with glucose. All diffraction peaks are indexed with the corresponding planes of CuO. No other peak due to possible impurities can be detected, which indicates that the products are of high purity. The XRD spectra showing the intense peak at 35.9 is having plane (111) which is the crystal plane of CuO. The low intensity peaks at 28.2, 42.3, 62.2, and 77.7 which match well with the plane (110), (202), (220) and (113). The peaks with 2θ values 25.12° and 28.76°confirmed that PANI coated Cu2O exhibit crystalline state (8).

 

Mortality rate of Artemia salina:

The Glu-CuO nanoparticle aggregates to elevated levels such that the guts were filled with particles showing significant mortality within 24 hours of exposure. The results were found to be in such a way that in the control the mortality was about 5.8% which was negligible. In minimum concentration of 0.05 mg/ml the mortality rate was 7.6%. About 46.46% and 76.3% of the population of Artemia salina were found to be dead as the concentration increased to the maximum in the test concentrations of 0.15 and 0.25 mg/ml. The LC50 value was obtained around 0.15 mg/ml concentration. And further extended exposure to 48 hours did induce high mortality. After 48 hours the mortality rate was twice the results of the 24-hour mortality rate and even in 0.05 mg/ml concentration about 22.8% mortality was observed. And the mortality was found to be above 82.6% at 0.15 mg/ml and 93% at 0.25 mg/ml concentration. However, these effects were most likely due to the lack of food uptake since the guts were completely filled with the aggregates of Glu-CuO nanoparticles (Table 1 and Figure 4). Maximum mortality rate was observed at 0.25 mg/ml concentration while 50 % mortality was observed at 0.15mg/ml concentration. The previous study suggested that the toxicity of silver nanoparticles to aquatic species depends on a concentration-dependent manner. This study reveals that the Glu-CuO nanoparticles have effect not only on the alive animal but also on cysts (9).

 

Morphological Variation of Artemia salina treated with Glu-CuO Nanoparticle

The aggregations of Glu-CuO nanoparticles inside the gut of Artemia salina were clearly observed under the phase contrast microscope and the images were photographed. As Artemia generally exhibits non-selective filter feeding behaviour, it consumes all particles that are below 50 microns in size. The amount of aggregation not only depends on the amount of concentration, but also depends on the amount of consumption of nanoparticles by each individual animal in various concentrations. In this study the Artemia salina were treated with various concentrations of Glu-CuO NPs such as 0.05, 0.15 and 0.25 mg/ml and after 48 hours of treatment they were observed under the phase contrast microscope and results were photographed. The results showed that in control the animal did not show any trace of aggregation; the mouth parts and the gut region appeared clear (Figure 5(a)). In minimum concentration (0.05 mg/ml) the aggregation of Glu-CuO nanoparticles was found around the mouth parts and some regions of the gut (Figure 5(b)), whereas in higher concentration (0.15 mg/ml), the entire gut region was accumulated with Glu-CuO nanoparticles (Figure 5(c)). And in maximum concentration (0.25 mg/ml) the gut was completely filled with Glu-CuO nanoparticle; due to the effect of high toxicity of Glu-CuO nanoparticles the tissue of the animal started to degrade (Figure 5(d)). Brine shrimps are non-selective filter feeders, and they can readily ingest particles of up to 50 μm in diameter (Simon 2006). When suspended in the seawater, these MO-NPs formed agglomerates that ranged from 400 nm up to several μm in diameter and the A. salina larvae were able to ingest them. Several studies have confirmed the accumulation of NPs inside the gut of A. salina larvae and their inability to eliminate these ingested particles (10, 11, 12).

 

Swimming Velocity:

Figure 6 shows that the average swimming velocities of A. salina were significantly affected by Glu-CuO NP compared to control. After 48 hrs exposure to 0.5 mg/ml, a decrease of 34 % of the swimming velocities was measured for A. salina. However at higher concentrations, the swimming velocity of A. salina was more impacted (65% and 75% for 1mg/ml and 1.5 mg/ml respectively).

 

Chemical analysis:

The total Glu-CuO nanoparticle contents of Artemia samples were determined by AF-MS. The concentration values were based on the wet weight of Artemia, reflecting the total body burden across the concentration 1mg/ml NP. Artemia larvae accumulated the aggregates of Glu-CuO NPs were shown in figure 7. The Cu levels accumulated within 48 h in larvae exposed to CuO nanoparticles were statistically different from the controls.

 

 

Figure 1: UV–visible absorbance spectral study of Cuo-NPs


 

Figure – 2: SEM images of CuO NPs

 

Figure-3: XRD result of CuO nanoparticles

 

Figure 4: Mortality rate of Artemia salina

 

Figure 5: Morphological variations of Artemia salina treated with Glu-CuO nanoparticle observed using Inverted phase contrast microscope

 

Figure 6: Mean swimming velocity in A. salina exposed to CuO NPs for 48 hr

 

Figure 7: Accumulation of NPs by A. salina larvae after 48 h of exposure to 1 mg/mL of Glu-CuO

 

Table 1: The Result for mortlity Rate (24 hrs& 48 hrs) of Brine shrimp Artemia Treated with various concentrations of Copper Nanoparticles

Parameter

Concentration levels in  (mg/ml)

Initial number of Artemia salina

Number of salina dead after 24 hours

Number of salina died after 48 hours

% of mortality after 24hours (mean±S)

% of mortality after 48 hours (mean±)

Mortality rate after

24 and 48

Hours

Control

13

1

8

7.69

61.53

0.3mg/ml

13

1

3

7.69

23.076

0.4mg/ml

13

6

7

46.15

53.846

0.5mg/ml

13

10

12

76.92

92.307

 


 

CONCLUSION:

In this study, we evaluated the stability of CuO NPs, and the toxic effects of their suspensions to Artemia salina larvae to elucidate the chemical and toxicological impact to marine micro-organisms. The results pointed to the fact that suspensions of CuO NPs were not acutely toxic to Artemia at environmentally feasible levels. However, prolonged exposure to the same suspensions induced significant toxicity. The results revealed that CuO NPs aggregate in seawater to micrometer particles. This process would ultimately reduce the toxic properties of the NPs. Nevertheless, CuO NPs showed differences in toxic effects depending on the concentration of nanoparticles. In future studies more attention should be given to the formulations of CuO NPs to better understand their toxicological properties since both surface properties and ion release kinetics change with underlying manufacturing processes. The exposure of these A. salina larvae to the selected MO-NPs did not induce significant mortality, although the NPs accumulated in the gut. However, behavioral and chemical analysis occurred after the exposure. The swimming speed alterations represent valid endpoints for CuO NP exposure.

 

REFERENCE:

1.       Kim KJ, Sung WS, Moon SK. Antifungal effect of silver nanoparticles on dermatophytes. Journal of Microbiology and Biotechnology. 2008; 18:1482–1484.

2.       Ashutoshkumar. Metal Oxide Nanoparticles Elicit Geno- toxic Responses in Mammalian Cells., Integral University, 2001

3.       Ravishankar Rai V. Nanoparticles and their potential application as antimicrobials. Science against microbial pathogen 2011.

4.       Jamuna Bai A. Nanoparticles and their potential application as antimicrobials. Science against microbial pathogen 2011.

5.       Shukla RK, Kumar A, Gurbani D, Pandey AK, Singh S; DhawanTiO(2) nanoparticles induce oxidative DNA damage and apoptosis in human liver cells. Nanotoxicology 7, (2003) 48-60.

6.       Yoshimura M, Namura S, Akamaysu H, Horio T. Antimicrobial  effects of phototherapy and photochemotherapy in vivo and in vitro. British Journal of Dermatology. 1994; 135: 528–532

7.       DhawanTiO(2) nanoparticles induce oxidative DNA damage and apoptosis in human liver cells. Nanotoxicology 7, (2003) 48-60.

8.       Stoimenov PK, Klinger RL, Marchin GL, 2005.Nanotoxicology: An emerging discipline evolving from studies of ultrafine particles. Environ. Health Perspect.

9.       Borkow G and J Gabbay (2009) Copper, An Ancient Remedy Returning to Fight Microbial, Fungal and Viral Infections. CurrChemBiol 3: 272-8.nce.

10.     Oberdorster G, Oberdorster E and Oberdorster J. 2005.Nanotoxicology: An emerging discipline evolving from studies of ultrafine particles. Environ. Health Perspect.

11.     Poland CA, Duffin R, Nee, WM and Donaldson, K. 2008. Carbon nanotubes introduced into the abdominal cavity of mice show asbestos like pathogenicity: In a pilot study. Nature Nanotechnology.

12.     Buzea, C., Pacheco, I. and Robbie, K. 2007. Nanomaterials andnanoparticles: Sources and Toxicity. Bio. Inter. Phases

 

 

 

 

 

Received on 20.03.2015                             Modified on 05.04.2015

Accepted on 10.04.2015      ©A&V Publications All right reserved

Res. J. Pharmacology & P’dynamics. 7(2): April- June 2015; Page 53-60